Introduction of Road maintenance joint sealant pavement crack sealant adhesive sealant for road crack repair
1. Product Description
Pavement crack sealant with hot-melt fast, strong adhesion, good anti-deformation recovery performance, can effectively seal pavement cracks and joints, and maintain sealing effect for a long time. Traffic can be restored after completion of construction.
Beijing Zhongtian Road-Tech Co.,Ltd ZT-PS Road pavement crack sealant for road crack repair performance index;
|
|
|
ow value(mm) |
Elastic recovery ratio/% |
Low temperature stretching |
|
|
Test temperature/ºC |
Maximum displacement/mm |
In conclusion |
High temperature type |
51 |
96 |
0 |
70 |
0 |
9.005 |
pass |
normal type |
69.10 |
92.60 |
1.87 |
62 |
-10 |
19.732 |
pass |
Low temperature type |
89 |
90.50 |
2.01 |
55 |
-20 |
45.600 |
pass |
Cold type |
108.30 |
87.40 |
2.65 |
48.1 |
-30 |
54.483 |
pass |
Severe cold type |
135 |
81 |
2.96 |
35 |
-40 |
62.123 |
pass |
From the above index, the indicators of ZT-PS Road pavement crack sealant for road crack repair meet and exceed the national & international technical standards. We master domestic leading road materials and new technologies, and some are at the international advanced level.
The product is divided into high temperature type, common type, low temperature type, cold type and cold type. To repair te cracks in asphalt pavements, the key is to choose a suitable type of sealant. According to different regions and different climatic conditions and pavement crack characteristics, choose the appropriate sealant as the material for pavement crack repair.
2. Beijing Zhongtian Road-Tech Co.,Ltd ZT-PS Road pavement crack sealant for road crack repair features;
1, High temperature does not flow, low temperature does not crack, good stability.
2, Resistance to water damage and aging resistance.
3, With strong adhesion and high elasticity.
4, The service life can reach 5 years.
5, Convenient and durable, environmentally friendly, can effectively extend the maintenance cycle, reduce the maintenance number of times.
3. Application:
Asphalt pavement crack
Concrete pavement crack
Bridges and parking Treatment crack
Cracks on the waterproof construction, etc.
4. User Guide
1. Before filling, ensure that the cracks are dry and there is no water or rain within 24 hours before and after potting.
2, according to customer requirements, whether to slotting and filling. The dust must be purged before potting.
3. When the temperature during the construction of the joint is lower than 5 °C, the crack should be preheated by a hot spray gun.
4. The filling joint is constructed by a filling machine with a stirring function. The sealing glue should be continuously stirred during the construction process. The sealing glue needs to be heated to 180-190 °C before the filling can be applied.
5, After the construction of the joint, it should be allowed to stand for 20 minutes to open the traffic. If it is open traffic immediately, it needs to sprinkle a small amount of fine sand or talcum powder, cement and other spacers to prevent the glue from sticking to the tire.
6. After the filling construction is completed, the sealing machine should be cleaned and the sealant should be avoided in the filling machine. After each section of the jointing construction, the filling machine should be cleaned.
5. Company Information
Zhongtian Road-Tech establishes a joint laboratory with Beihang University, and has two production bases in Hebei, with an annual output of 60,000 tons of rubber asphalt, 2,000 tons of HVA high viscosity modifier, 3,000 tons of anti-rutting agent, 5,000 tons of sealant.
We wins more than 30 patents and formulates 8 standards for China's transportation industry. The leaders win the China National Science and Technology Progress Award and enjoy a high reputation in the industry.
6. Certificates & Honor
Beijing Zhongtian Road-Tech Co.,Ltd. is the Board of Directors of China Transportation Association and Transportation Committee of China Technological Market Association, with expert technical R&D team, continuous innovation ability, rich engineering experience and sufficient capacity. Also we participated in designated road material industry standard certificates.
Beijing Zhongtian Road-Tech Co., Ltd. is a professional road asphalt material and equipment manufacturer.
7. Application Cases
1, Welcome customers to come to our factory for inspection. (we have a joint laboratory with Beihang University, and has two production bases in Hebei)
2, We are not afraid to compare performance with similar products. ( we masters domestic leading road materials and new technologies, and some are at the international advanced level)
3, Welcome customers to our engineering case to do on-site inspection. (Our products have been applied in major engineering projects at home and abroad, including Chang'an Avenue, the China's National First Road, Beijing Third Ring Road, Ethiopian AA highway pavement, etc. They're highly recognized by customers.)